Key points

From the paper's conclusion
  • High‐performance glycerol‐based urethane acrylate (UA) photopolymers were synthesized by reacting toluene diisocyanate (TDI) with 2‐hydroxyethyl methacrylate (HEMA) at a 1:1 M ratio, followed by reaction with glycerol.

Abstract

High‐performance glycerol‐based urethane acrylate (UA) photopolymers were synthesized by reacting toluene diisocyanate (TDI) with 2‐hydroxyethyl methacrylate (HEMA) at a 1:1 M ratio, followed by reaction with glycerol. The formulations were designed as G1, G2, and G3 classes according to the targeted participation of one, two, or three glycerol hydroxyl groups, respectively, while dipropylene glycol diacrylate (DPGDA) was used as a reactive diluent. In selected G3‐class formulations, bisphenol A ethoxylate diacrylate (BisA‐DA) was incorporated to assess the influence of aromatic rigidity and ether flexibility. The resins were processed by LCD‐type 3D printing and systematically characterized. FTIR and 1 H NMR analyses indicated that these classes contained distributions of substitution states rather than single, fully substituted species. Mechanical performance was strongly influenced by the type and relative proportion of the glycerol‐based urethane acrylate structures, the DPGDA content, and the presence or absence of BisA‐DA. G3‐65 reached a tensile strength of 80.7 MPa, G2‐75 reached 82.7 MPa, and BIS6.25 reached 88.2 MPa, while BIS12.5 showed an elongation at break of 14.8% and an impact resistance of 12.7 kJ/m 2 . These values are among the highest reported for vat‐photopolymerized resin systems and indicate a strong combination of strength, toughness, and ductility. DSC analysis showed a broad and weak glass‐transition region between 57.5°C and 78.1°C, indicating restricted segmental mobility in the cured networks. TGA results showed formulation‐dependent thermal stability, with T 5 values (temperature at 5% weight loss) ranging from 260°C to 295°C and maximum weight‐loss temperatures reaching up to 416°C. SEM images reveal densely packed phase microdomains resembling network‐like structures, which are consistent with the improved mechanical performance of these formulations.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Development of High‐Performance Polymers via Curing of Glycerol‐Based Photoresins — Science Skim