Top‐ and bottom‐of‐the‐line corrosion: Effects of 30 °C bottom liquid and 20 °C steel temperature in CO 2 and H 2 S/N 2 environments
M. Taqiuddin, N. Kamil Othman, A. Md Noor, N. Yaakob
Key points
From the paper's conclusion- This study examines the corrosion behavior of API 5L X65 carbon steel under top (TLC) and bottom (BLC) conditions in sweet (CO 2 ) and sour (H 2 S/N 2 ) environments at 20 °C – 30 °C.
Abstract
Corrosion in oil and gas pipelines is strongly influenced by environmental chemistry and pipeline location, affecting reliability and safety. This study examines the corrosion behavior of API 5L X65 carbon steel under top (TLC) and bottom (BLC) conditions in sweet (CO 2 ) and sour (H 2 S/N 2 ) environments at 20 °C – 30 °C. Uniform corrosion rates (UCR) and pitting corrosion rates (PCR) were measured using weight loss (ASTM G1‐03) and surface profilometry (ASTM G46‐21), while scanning electron microscopy (SEM), energy dispersive x‐ray spectroscopy (EDX) and x‐ray diffraction (XRD) characterized surface morphology and corrosion products. In the sweet environment, top‐of‐the‐line corrosion and bottom‐of‐the‐line corrosion showed similar uniform corrosion rates (0.28 mm/y). Pitting corrosion was moderate, with pitting corrosion rates of 0.89 mm/y for top‐of‐the‐line corrosion and 0.67 mm/y for bottom‐of‐the‐line corrosion. Products were mainly thin Fe 3 C layers, with NaCl deposition only at the bottom. Under sour conditions, bottom‐of‐the‐line corrosion exhibited higher uniform corrosion rates (0.29 mm/y) than top‐of‐the‐line corrosion (0.22 mm/y), with more severe localized corrosion; pitting corrosion rate reached 1.94 mm/y at bottom‐of‐the‐line corrosion versus 0.43 mm/y at top‐of‐the‐line corrosion. Multilayered FeS scales formed in H 2 S environments, partially protecting the top, while bottom surfaces experienced combined sulfide and chloride attack, promoting localized pitting. These findings show that pipeline corrosion depends strongly on chemical environment and steel position, emphasizing the need for localized monitoring and targeted mitigation strategies to maintain pipeline integrity.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Top‐of‐line corrosion in marginal sour environment: protectiveness of iron (II) sulphide in wet gas pipelineMaterialwissenschaft und Werkstofftechnik · 2026
- A Mechanistic Model for Predicting Top‐of‐the‐Line Corrosion in CO₂ /H₂ S Environments: Validation and Field ApplicationMaterials and Corrosion · 2026
- Effects of Water Content on the Pitting Behavior of X65 Steel in Supercritical and Dense-Phase Carbon Dioxide EnvironmentsMetals · 2026
- Study on the effects of hydrostatic pressure, temperature and oxygen content on the electrochemical corrosion of 20# steelAnti-Corrosion Methods and Materials · 2026
- Surface chemistry of carbon steel in contact with CO2 streams containing impuritiesCorrosion Science · 2026
- Galvanic corrosion behavior of X80 pipeline steel welded joint in three representative soil environmentsJournal of Materials Research and Technology · 2026