Hamidreza M. Shirazi, Taegen M. Poles, Fei Long, Kevin Daub, Jason D. Giallonardo, Peter G. Keech, Desmond C. Williams, Roger C. Newman,
Key points
From the paper's conclusion- The present work investigates the tensile behavior of a copper coating electrodeposited onto steel that had been prepared in an acid bath after heat treatment.
Abstract
The present work investigates the tensile behavior of a copper coating electrodeposited onto steel that had been prepared in an acid bath after heat treatment. The copper is brittle at slow strain rates (1 × 10 −6 s −1 ) but ductile at fast strain rates (1 × 10 −3 s −1 ). A uniform distribution of tiny cavities is observed throughout the material after electrodeposition. Microstructural and chemical composition characterizations demonstrate that annealing the electrodeposited copper at 600°C increases grain size and transitions the morphology adjacent to the copper‐steel deposition interface from lamellar to equiaxed. Approximately 32% of the initial 17.8 ± 4.0 wppm hydrogen content is released by the 600°C annealing. Nano‐analysis of annealed samples shows the redistribution and the coalescence of cavities at grain boundaries, twins, and dislocations. Slow strain rate (1 × 10 −6 s −1 ) tensile tests of 600°C annealed samples still show a significant strain rate sensitivity, similar to the non‐heat‐treated material, and only a small improvement in ductility. Redistribution of solute hydrogen atoms on dislocations during annealing is hypothesized to be the reason behind this phenomenon.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Hollow specimen method for tensile tests in high-pressure hydrogen gas: The role of strain rate and surface qualityMRS Bulletin · 2026
- Mechanical properties of SS310 and IN625 following high-temperature hydrogen exposureFrontiers in Energy Research · 2026
- The Effect of Cu-Rich Nano-Precipitation on Hydrogen Embrittlement Performance in a Cu-Bearing Ultra-Low Carbon Steel.Materials (Basel, Switzerland) · 2026
- Compatibility of cold drawn and heat treated austenitic stainless steel (316L) tube for green hydrogen applicationsWelding in the World · 2026
- Transient Hydrogen-Manipulated Nonequilibrium Kinetics of Abnormal Grain Growth for Single-Crystal Copper Foils.ACS applied materials & interfaces · 2026
- Hydrogen embrittlement susceptibility of AA7075 aluminum alloy subjected to continuous retrogression and re-aging treatment in an aggressive acidic chloride environmentDiscover Materials · 2026