Long‐Term Corrosion of Carbon‐Steel Casing Used in Deep Geological Radioactive Waste Repository
Mahado Saïd Ahmed, Delphine Neff, Annabelle Vernouillet, Xavier Bourbon, Didier Crusset, Gaëlle Charrier, Valérie Maillot, Philippe Dillmann
Key points
From the paper's conclusion- The study examines the 6‐year corrosion of carbon‐steel casing in Andra's deep geological repository (Bure, France), where steel pipes are embedded in cementitious filling grout (CFG) within Callovo‐Oxfordian claystone.
Abstract
The study examines the 6‐year corrosion of carbon‐steel casing in Andra's deep geological repository (Bure, France), where steel pipes are embedded in cementitious filling grout (CFG) within Callovo‐Oxfordian claystone. Samples from 0.28, 6, and 15 m depths revealed three corrosion patterns: Type I (Fe(III) oxyhydroxides like goethite, persisting from atmospheric pre‐corrosion), Type II (Fe(II)/Fe(III) phases like magnetite and iron sulfides, indicating deaeration), and Type III (minimal corrosion), likely due to abrasion or limited pre‐exposure. CFG saturation, Cox water ingress, and cell geometry (e.g., Viking seal) drove spatial variability. No significant CPL thickness increase was observed, suggesting limited corrosion progression under most conditions. The atmospheric pre‐corrosion layer acted as a marker of local redox states, while saturated, confined zones promoted magnetite and sulfide formation. This work highlights the heterogeneity of corrosion in geological repositories and the need to account for local environmental factors in long‐term safety assessments.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Integrated Corrosion Assessment of Copper Canisters for Deep Geological Disposal in Crystalline Rock: A Case Study in TaiwanMaterials and Corrosion · 2026
- Current Development of Geological Disposal Facilities: A Comprehensive Review of Corrosion and Microbially Influenced Corrosion of Nuclear Waste Canisters.Materials (Basel, Switzerland) · 2026
- Corrosion Monitoring of Metal Components in the Beishan Underground LaboratoryMaterials and Corrosion · 2026
- Effect of bentonite form on the corrosion behavior of copper for high-level nuclear waste disposal canisterJournal of Materials Research and Technology · 2026
- Galvanic Corrosion Behavior Between Copper (T2) and Carbon Steel (Q235) in Simulated Deep Geological EnvironmentJournal of The Electrochemical Society · 2026
- Potential Influence of Microorganisms on the Corrosion of Carbon Steel in the French High‐Level, Long‐Lived Radioactive Waste Disposal Context at 30°CMaterials and Corrosion · 2026