Immobilization of Pb and Zn from mining waste using alkali‐activated materials: Physico‐chemical properties and leaching behavior
Yamina Romdhani, Samir Mefteh, Mahdi Hdidar, Mabrouk Ben Hamden, Lamiae El Alaoui, Abdelaziz Sebei, Rui M. Novais, Slavka Andrejkovičová,
Key points
From the paper's conclusion- The results showed that high waste contents (>50 wt%) or low alkaline activator concentrations led to poor mechanical and physico‐chemical properties.
Abstract
The management of mining waste containing potentially toxic elements represents a major environmental concern. In this study, mining residues from the Boujaber abandoned Pb–Zn mine (northwest Tunisia) were valorized through alkali activation in order to develop environmentally safe construction materials. Mining waste was used as a partial replacement for metakaolin in the synthesis of alkali‐activated materials. Different formulations were prepared using sodium hydroxide solutions with concentrations ranging from 6 to 12 M and cured for up to 28 days. The materials were characterized in terms of compressive strength, Fourier‐transform infrared spectroscopy (FTIR), apparent density, water absorption, and microstructure (SEM). Particular attention was given to the immobilization of potentially toxic elements through leaching tests. The raw mining waste exhibited high concentrations of hazardous elements, especially Pb (3710 ppm) and Zn (14,860 ppm). The results showed that high waste contents (>50 wt%) or low alkaline activator concentrations led to poor mechanical and physico‐chemical properties. Conversely, formulations incorporating ≤50 wt% mining waste and activated with 10–12 M NaOH demonstrated improved performance. Leaching tests confirmed the effective immobilization of Zn within the alkali‐activated matrix, while Pb leaching was significantly reduced but remained above the NT 106.002 limit (0.1 mg/L), although still compliant with the less restrictive USEPA threshold (5 mg/L), indicating partial immobilization of this element. Among the tested formulations, the 80% metakaolin–20% mining waste composition showed the most advantageous performance, combining the highest compressive strength with the lowest Pb and Zn leaching concentrations, in compliance with regulatory limits, while offering a cost‐effective and environmentally beneficial valorization of mining waste. This study highlights the potential of alkali‐activated materials as a sustainable solution for the stabilization and reuse of mining waste, contributing to both environmental protection and resource efficiency.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- In-situ formation of LDH/zeolite nanocrystals in alkali-activated materials for efficient lead-zinc tailings stabilization.Environmental research · 2026
- Sustainable valorization of copper mine waste into construction materials by alkali activationScientific Reports · 2026
- Hydrometallurgical Zinc Recovery from Municipal Solid Waste Incineration Boiler Fly Ash and Mechanical Performance of Ceramic Materials Developed from the Leaching ResidueApplied Sciences · 2026
- Towards eco-friendly mining: Alkali-activated materials from mine waste for pollution mitigationGreen and Smart Mining Engineering · 2026
- Heavy metals incorporated-alkali-activated waste glass binder and foamed glass: phase composition, physicomechanical performance, and reaction mechanism.Scientific reports · 2026
- Characterisation of copper mine tailings for environmental stability from the Copperbelt Province, Zambia.Environmental monitoring and assessment · 2026