Journal of Applied Polymer Science

Carbon Fiber Felt Reinforced TaC ‐ LaB 6 /Silicone‐Modified Phenolic Aerogel Composites: Lightweight, Low Shrinkage and Enhanced Ablation Resistance

Xinzhe Shi, Xin Liu, Bing Wang, Bowen Li, Zhixiong Huang, Yanbing Wang

Key points

From the paper's conclusion
  • Overall, considering the comprehensive balance of low density, mechanical properties, and ablation resistance, the CSiPR‐3 sample (50% filler) exhibits the best overall performance.

Abstract

A carbon fiber felt was introduced as a 3D reinforcement skeleton. TaC‐LaB 6 nano‐ceramic fillers were added synergistically. A series of ceramizable aerogel composites were successfully prepared. The results show that the composites remain lightweight (density 0.305–0.436 g/cm 3 ). Their volume shrinkage after drying is as low as about 0.6%. The composites exhibit obvious anisotropy. The ceramic fillers significantly improve high‐temperature stability. As the ceramic filler content increases, the high‐temperature stability improves significantly. In air at 1000°C, the mass retention rate increases from 60.18% to 81.90%. Meanwhile, the linear ablation rate decreases from 0.072 to 0.041 mm/s. Overall, considering the comprehensive balance of low density, mechanical properties, and ablation resistance, the CSiPR‐3 sample (50% filler) exhibits the best overall performance. During ablation, TaC and LaB 6 undergo a series of reactions. They finally form a dense composite protective layer. This layer consists of Ta 2 O 5 , LaTaO 4 , and a borosilicate glass phase. It effectively blocks the erosion of heat flow and oxygen.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Carbon Fiber Felt Reinforced TaC ‐ LaB 6 /Silicone‐Modified Phenolic Aerogel Composites: Lightweight, Low Shrinkage and Enhanced Ablation Resistance — Science Skim