Thermo‐Alkaline Coupled Aging of Modified Polytetrafluoroethylene Gaskets in Alkaline Water Electrolysis: Failure Behavior Analysis
Chuanhao Liu, Huan Yao, Yirui Lu, Hong lv, Daijun Yang
Key points
From the paper's conclusion- These findings describe the response of the tested material at the selected temperatures and under the specified exposure protocol, providing reference data on material properties relevant to sealing applications.
Abstract
Sealing gaskets are critical to alkaline water electrolysis (AWE) systems, yet their thermo‐alkaline degradation remains insufficiently quantified. Modified polytetrafluoroethylene (m‐PTFE) composite gaskets were aged in 30 wt% KOH for 168 h at 20°C, 60°C, 90°C, 120°C, and 150°C. For this commercial composite, 90°C was the first tested temperature showing a marked decrease in displacement‐based elongation at break, from 157.61% ± 7.08% to 108.87% ± 3.88%. Tensile strength decreased numerically at 20°C, while recovery ratio and tensile strength increased numerically at 150°C relative to 120°C; these pairwise differences were not statistically significant after Holm adjustment. Differential scanning calorimetry located pristine‐composite melting above the aging range, while Fourier transform infrared spectroscopy showed retention of dominant PTFE bands. Thermogravimetric analysis revealed lower temperatures for 5% mass loss after aging. External‐surface scanning electron microscopy–energy dispersive X‐ray spectroscopy revealed cavities, surface heterogeneity, and increased constituent exposure. Morphological evolution and possible changes in interfacial interactions and load sharing offer a potential explanation for the observed mechanical response. These findings describe the response of the tested material at the selected temperatures and under the specified exposure protocol, providing reference data on material properties relevant to sealing applications.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Atomic Layer Deposited Zirconium Dioxide/PTFE Separators for Intermediate‐Temperature Alkaline Water Electrolysis: In Situ CharacterizationChemie Ingenieur Technik · 2026
- Creep Mechanical Performance of Cryogenically Aged PTFE at Room TemperatureCryo · 2026
- 2000 kW Alkaline Water Electrolyzer: Stability Evaluation of Electrodes and Separators After a Seven-Year Long-Term RunEnergy & Fuels · 2026
- Coupled thermo–hygro–mechanical ageing and chemical degradation mechanisms of polyurethane adhesive joints in bus structures: glass bondingJournal of Adhesion Science and Technology · 2026
- Study on the Multi‐Environment Anti‐Aging Performance of Nano‐Textured PTFE – Al 2 O 3 Hybrid FKM CompositesJournal of Applied Polymer Science · 2026
- Long‐Term Durability Modeling of GFRP Rebar Under Natural and Accelerated Alkaline Conditioning Using Logarithmic Regression and Time–Temperature SuperpositionPolymer Composites · 2026