Angewandte Chemie (International ed. in English)

Balancing pH Mismatch in Electrolytic Zn-MnO2 Batteries via a Synergetic Anion-Proton Interactive Electrolyte.

Peiyan Tong, Mingming Wang, Shunxin Tan, Dongyang Shen, Ruihao Luo, Taoli Jiang, Guili Zhao, Hongxu Liu,

Department of Applied Chemistry, School of Chemistry and Materials Science, Hefei National Research Center for Physical Sciences At the Microscale, University of Science and Technology of China, Hefei, Anhui, China. · Zhejiang Key Laboratory of Intelligent Manufacturing For Functional Chemicals, ZJU-Hangzhou Global Scientific and Technological Innovation Center, Zhejiang University, Hangzhou, China.

Key points

From the paper's conclusion
  • In this study, a synergetic anion-proton interactive (SAPI) electrolyte regulation strategy is reported to balance the pH mismatch, which can not only regulate the electrode-electrolyte interfacial microenvironment to promote the deposition of highly (002)-oriented Zn plane with high resistance to the hydrogen evolution reaction and corrosion on anode, but also accelerate the redox reaction of MnO

Abstract

Electrolytic Zn-MnO2 batteries (EZMBs) are considered a promising technology for grid-scale energy storage due to their low cost, high specific capacity, high operating voltage and safety. However, the tradeoff between the mildly acidic environment for high-efficiency zinc deposition on anode and the high concentration of protons required to trigger the MnO2/Mn2+ conversion reaction on cathode leads to the pH mismatch issue, finally causing the instability and short lifespan of current EZMBs. In this study, a synergetic anion-proton interactive (SAPI) electrolyte regulation strategy is reported to balance the pH mismatch, which can not only regulate the electrode-electrolyte interfacial microenvironment to promote the deposition of highly (002)-oriented Zn plane with high resistance to the hydrogen evolution reaction and corrosion on anode, but also accelerate the redox reaction of MnO2/Mn2+ conversion on cathode, simultaneously. As a result, the SAPI electrolyte enables a 40-fold lifespan enhancement of over 5000 cycles at a current density of 10 mA cm-2 in Zn-Zn symmetric cells as compared to the pristine electrolyte. Furthermore, the EZMBs in SAPI electrolyte achieve an elevated average discharge voltage of 0.4 V and about 10-fold stable cycling lifespan than the pristine one. This strategy provides novel insights into designing long-life EZMBs and orientational deposition of zinc anode.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.