Advanced Energy Materials

Ultra‐High Ionic Conductivity Sulfide‐Based Composite Membranes Paired With Stable Interfacial Layer Enables High‐Energy‐Density All‐Solid‐State Batteries

Yang Li, Jiachen Hu, Huan Li, Xianyi Zhao, Peng Lei, Xiaoxue Zhao, Hong Liu, Ce‐Wen Nan,

Key points

From the paper's conclusion
  • A high-performance sulfide solid-state electrolyte (Li5.4PS4.4Cl0.8Br0.8) was combined with Polytetrafluoroethylene binder to create a high-ionic-conductivity composite membrane (HICCM).
  • The HICCM paired with a LiF-rich interfacial layer enables stable cycling for 2000 hours at 0.2 mA cm-2 and achieves an energy density of 416.5 Wh kg-1 at 3.4 mAh cm-2.
  • This work demonstrates that combining HICCM with a stable interface design can enable high-energy-density and long-lasting all-solid-state batteries.

Abstract

Intrinsic properties of sulfide solid‐state electrolytes (SEs) are crucial for achieving all‐solid‐state batteries (ASSBs) with high safety and high energy density, yet it is challenging to fabricate high‐performance sulfide SE films in a scalable approach. Furthermore, the inevitable side reactions between sulfide SE and lithium metal anodes exacerbate interfacial incompatibility, causing degradation in the cyclic stability. Here, a high‐performance sulfide SE (Li 5.4 PS 4.4 Cl 0.8 Br 0.8 ) was selected as the base phase to compensate for the loss of electrochemical performance during the dry film‐forming process. It was then combined with Polytetrafluoroethylene binder to prepare a high‐ionic‐conductivity composite membrane (HICCM). To mitigate side reactions between HICCM and the anode, a LiF‐rich interfacial layer forms in situ on the lithium metal surface, and the assembled symmetric cell achieves a high critical current density of 1.3 mA cm −2 and stable cycling for 2000 h (0.2 mA cm −2 ). For electrochemical performance, HICCM exhibits fast ion transport kinetics and electrical insulation, allowing the ASSB configured as FeS 2 //HICCM//LiF‐Li to achieve an energy density of 416.5 Wh kg −1 at a high loading of 3.4 mAh cm −2 . This work demonstrates that by combining HICCM with a stable interface design, ASSBs can achieve longevity and high cell‐level energy density.

Read the paper

Discussion · 1

Science Skim's AI key points, plus readers' public thoughts

Science SkimAI key points
Pinned
  • A high-performance sulfide solid-state electrolyte (Li5.4PS4.4Cl0.8Br0.8) was combined with Polytetrafluoroethylene binder to create a high-ionic-conductivity composite membrane (HICCM).
  • The HICCM paired with a LiF-rich interfacial layer enables stable cycling for 2000 hours at 0.2 mA cm-2 and achieves an energy density of 416.5 Wh kg-1 at 3.4 mAh cm-2.
  • This work demonstrates that combining HICCM with a stable interface design can enable high-energy-density and long-lasting all-solid-state batteries.