Clean Thermolysis PMMA Top Layer Enables High-Efficiency Kesterite Solar Cells.
Rilige Su, Lingling Wang, Yawei Wang, Hao Li, Rui Guo, Xingyu Lu, Xinghang Niu, Ning Xia,
State Key Laboratory of Integrated Optoelectronics, Key Laboratory of UV Light-Emitting Materials and Technology of Ministry of Education, School of Physics, Northeast Normal University, Changchun, Jilin, China. · Chongqing Key Laboratory of Interface Physics in Energy Conversion, School of Physics, Chongqing University, Chongqing, China.
Key points
From the paper's conclusion- This work demonstrates a simple yet effective interfacial engineering strategy for steering selenization pathways, offering a practical route toward higher-quality kesterite absorbers.
Abstract
Regulating the phase evolution during selenization of kesterite (Ag,Cu)2ZnSn(S,Se)4 (ACZTSSe) absorbers is essential for high-efficiency solar cells, yet it remains challenging because of uncontrolled contact reactions between the precursor film and selenium vapor. Herein, we introduce a poly (methyl methacrylate) (PMMA) blocking layer with clean-thermolysis characteristics onto the ACZTSSe precursor top surface to precisely control the onset of selenization. At low temperatures, the PMMA layer acts as a physical barrier that isolates the precursor from Se vapor, effectively suppressing premature reactions and secondary phase formation. Upon heating above 400°C, the PMMA decomposes almost residue-free, immediately exposing the precursor to high-concentration Se vapor and triggering a rapid one-step conversion into the desired kesterite phase. This temperature-triggered decomposition decouples early-stage intermediate reactions from final phase formation, significantly reducing secondary phases and the density of detrimental [2CuZn+SnZn] defect clusters. Variable-wavelength photoluminescence confirms the simultaneous suppression of non-radiative recombination in both the bulk and the interfaces, yielding a prolonged minority carrier lifetime. The optimized device achieves a power conversion efficiency of 14.69% with an open-circuit voltage of 566 mV. This work demonstrates a simple yet effective interfacial engineering strategy for steering selenization pathways, offering a practical route toward higher-quality kesterite absorbers.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Buried CdSe Sacrificial Layer Driving Phase Evolution and Crystallization Kinetics Enables 14.78%-Efficient DMF-Based Kesterite Solar Cells.Advanced materials (Deerfield Beach, Fla.) · 2026
- Multiple Synergistic Effects Enabling Efficient Kesterite Solar Cells via Introducing a Cu 2 O‐Bi 2 O 3 Sacrificial InterlayerCarbon Energy · 2026
- Small Molecule Thiol Self-Assembled Interlayer Enhances Carrier Extraction at CZTSSe/CdS Interface for High Efficiency Photovoltaics.ACS applied materials & interfaces · 2026
- Engineering of Heterogeneous Redox Environment Enables Balanced Phase Evolution and Nucleation for 14.4% Efficiency CZTSSe Solar CellSmall · 2026
- Buried Interface Modulation Enables Efficient CZTSSe Solar Cells on Transparent SubstratesAdvanced Functional Materials · 2026
- Rapid Cooling After Device Annealing Suppresses Interface Losses in Cu2ZnSnS4 Solar Cells Enabling High Efficiency and Stability.Advanced science (Weinheim, Baden-Wurttemberg, Germany) · 2026