Advanced science (Weinheim, Baden-Wurttemberg, Germany)

Ultra-Wide Temperature-Stable High Piezoelectricity in Textured CaBi2Nb2O9 Ceramics via Defect-enhanced Asymmetric Jahn-Teller Distortion.

Xiaogang Luo, Xuefan Zhou, Yan Zhang, Hang Luo, Xi Yuan, Dou Zhang

College of Chemistry and Chemical Engineering, Central South University, Changsha, Hunan, China. · Powder Metallurgy Research Institute, State Key Laboratory of Powder Metallurgy, Central South University, Changsha, Hunan, China.

Key points

From the paper's conclusion
  • In this work, the CuO doping strengthens the structural rigidity of the octahedral network against temperature by coupling the Jahn-Teller effect of Cu2+ with defect dipoles to form a defect-enhanced Jahn-Teller distortion, combined with the modulation of the polarization to the poling electric field direction via textural engineering, significant improvement of both piezoelectric response and tem

Abstract

CaBi2Nb2O9 is regarded as an eminently promising candidate for high-temperature piezoelectric devices due to its ultra-high Curie temperature and good insulation. Unfortunately, extremely low piezoelectric properties and poor temperature stability severely hinder its practical application. In this work, the CuO doping strengthens the structural rigidity of the octahedral network against temperature by coupling the Jahn-Teller effect of Cu2+ with defect dipoles to form a defect-enhanced Jahn-Teller distortion, combined with the modulation of the polarization to the poling electric field direction via textural engineering, significant improvement of both piezoelectric response and temperature stability can be realized simultaneously. As a result, the sample with 0.1 wt.% CuO not only maintains an ultra-high Curie temperature (TC ∼ 958°C) but also exhibits a d33 value of ∼27 pC/N and a low high-temperature (600°C) dielectric loss of 0.028. Simultaneously, its piezoelectric properties demonstrated excellent temperature stability by in-situ heating up to 600°C (Δd33∼4.96%) as well as undergoing 10 cycles of high-low temperature cycling tests (RT-750°C-RT, enduring approximately 240 h). This work represents a breakthrough for the practical application of high-temperature piezoelectric ceramics.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts