Advanced science (Weinheim, Baden-Wurttemberg, Germany)

Synergistic Effects of Separator Architecture and Electrolyte Chemistry on the Electrochemical Stability of Lithium Ion Batteries With Li-Mn Rich Cathodes and µ-Si Anodes.

Marian Cristian Stan, Bärbel Arling, Gerrit Michael Overhoff, Kirstin Darida, Lucas Marquart, Peng Yan, Lara Kersting, Linus Voigt,

Institute of Energy Materials and Devices, Helmholtz Institute Münster: Ionics in Energy Storage (IMD-4 / HI MS), Forschungszentrum Jülich GmbH, Münster, Germany. · MEET Battery Research Center, University of Münster, Münster, Germany.

Key points

From the paper's conclusion
  • The capacity fading behavior of LMR||µ-Si cells was studied by comparing conventional polyolefin Celgard 2500 separators with an electrospun polyacrylonitrile (PAN) membrane.
  • Cells with Celgard separators exhibit rapid degradation, with capacity roll-over occurring after less than 75 cycles, while PAN membrane-enhanced cells retain 80% of the initial capacity after approximately 230 cycles.
  • These findings highlight the synergistic influence of separator selection and electrolyte formulation in stabilizing interphases at both electrodes.

Abstract

High-voltage, high-capacity lithium ion batteries (LIBs) combining cobalt-free lithium manganese-rich (LMR) cathodes with pure silicon (µ-Si) anodes offer a promising route toward more sustainable and cost-effective energy storage. In this study, the capacity fading behavior of LMR||µ-Si cells is correlated with the poor wettability of the conventional polyolefin Celgard 2500 separator, which leads to non-uniform electrolyte distribution and localized Li metal deposition on the µ-Si surface. Consequently, cells with Celgard separators exhibit rapid degradation, with capacity roll-over occurring after less than 75 cycles. In contrast, replacing Celgard 2500 with an electrospun polyacrylonitrile (PAN) membrane enhances cycling stability, retaining 80% of the initial capacity after approximately 230 cycles, due to improved electrolyte wetting and mechanical contact with µ-Si anode. Further optimization of the electrolyte composition, using N, N-dimethylsulfamoyl fluoride (DMFSA) as co-solvent with fluoroethylene carbonate (FEC), extends LMR||µ-Si cell lifetime to more than 400 cycles, regardless of the separator type. These findings highlight the synergistic influence of separator selection and electrolyte formulation in stabilizing interphases at both electrodes. A holistic materials design approach is therefore essential for advancing the performance and durability of next-generation LMR||µ-Si-based LIBs cells.

Read the paper

Discussion · 1

Science Skim's AI key points, plus readers' public thoughts

Science SkimAI key points
Pinned
  • The capacity fading behavior of LMR||µ-Si cells was studied by comparing conventional polyolefin Celgard 2500 separators with an electrospun polyacrylonitrile (PAN) membrane.
  • Cells with Celgard separators exhibit rapid degradation, with capacity roll-over occurring after less than 75 cycles, while PAN membrane-enhanced cells retain 80% of the initial capacity after approximately 230 cycles.
  • These findings highlight the synergistic influence of separator selection and electrolyte formulation in stabilizing interphases at both electrodes.

Readers' thoughts

No reader thoughts yet.