Triple-Coupling Regulation Enables Dendrite-Free Subzero Aqueous Zn-Ion Batteries.
Mengyang Dong, Zhibao Yang, Lina Pan, Jie Qu, Shangshu Qian, Jessica Hamilton, Bernt Johannessen, Yuhui Tian,
College of Chemistry and Chemical Engineering, Hunan Normal University, Changsha, China. · College of Chemical and Biological Engineering, Zhejiang University, Hangzhou, China.
Key points
From the paper's conclusion- Aqueous Zn-ion batteries (AZIBs) suffer severe degradation at subzero temperatures due to electrolyte freezing, sluggish Zn2+ kinetics, and dendrite-induced interfacial instability.
Abstract
Aqueous Zn-ion batteries (AZIBs) suffer severe degradation at subzero temperatures due to electrolyte freezing, sluggish Zn2+ kinetics, and dendrite-induced interfacial instability. Herein, a triple-coupling regulation strategy integrating solvation structure, interfacial chemistry, and crystallographic orientation through a formamide-ethanol deep eutectic electrolyte (ZEFW2) was developed. Molecular dynamics simulations and spectroscopic analyses reveal that ZEFW2 redistributes the primary Zn2+ solvation environment, reducing H2O and acetate coordination while introducing formamide coordination and maintaining favorable Zn2+ transport. Depth-resolved XPS further reveals a chemically reconstructed Zn interphase containing Zn-O-related inorganic species and persistent N- and C-containing electrolyte-derived species. The modified solvation and interfacial environments regulate Zn nucleation and promote preferential Zn deposition along the (101) facet, enabling more homogeneous Zn growth and suppressing dendritic morphology. Consequently, Zn||Zn symmetric cells achieve 1400 h of cycling at -20°C under 1 mA cm-2 and 10 mAh cm-2, with a Coulombic efficiency of 99.78% over 1200 cycles. Zn||NVO full cells retain 74% of their initial capacity after 1600 cycles at -20°C, while pouch cells demonstrate stable operation at both room and subzero temperatures. This work establishes a molecular-to-interfacial triple-coupling strategy for temperature-resilient AZIBs.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Synergetic Regulation of Enthalpy‐Entropy via Dipole Interactions Enabling Textured and Low‐Temperature Aqueous Zinc‐Ion BatteriesAdvanced Energy Materials · 2026
- Strategies for Designing Cryogenic Aqueous Zinc‐Ion Batteries: From Electrode Engineering to Electrolyte OptimizationChemElectroChem · 2026
- Gradient chaotropic regulation of Zn2+ solvation chemistry for low-temperature zinc metal batteriesNature Communications · 2025
- Multivariate Competitive Coordination Structure in Hydrated Eutectic Electrolytes for Ultra‐Long Low‐Temperature Aqueous Zinc‐Ion ElectrochemistryAdvanced Energy Materials · 2025
- Advanced electrolytes for low-temperature zinc-ion batteriesPhilosophical Transactions of the Royal Society A Mathematical Physical and Engineering Sciences · 2026
- Dual-solvent mediated solvation-to-interphase coupling enables durable wide-temperature aqueous zinc ion batteries.Journal of colloid and interface science · 2026