Synergistic Regulation of Deep-Cycling-Induced Zn Pulverization and Resting Galvanic Corrosion in Practical Lean Zinc Anodes.
Jing Xu, Haolin Li, Qiyin Jing, Lingfei Zhao, Elad Ballas, Bing Sun, Doron Aurbach, Guoxiu Wang
Research Center of Grid Energy Storage and Battery Application, School of Electrical and Information Engineering, Zhengzhou University, Zhengzhou, China. · Centre for Clean Energy Technology, School of Mathematical and Physical Sciences, Faculty of Science, University of Technology Sydney, New South Wales, Australia.
Key points
From the paper's conclusion- Benzotriazole (BTA) is introduced as an electrolyte additive in ZnSO4 electrolytes to modify the electric double layer on the Zn anode.
- BTA alleviates the mismatch between Zn2+ transport and reduction kinetics, forming dense zinc deposits and reducing pulverization.
- BTA also blocks electron transfer pathways on the Cu substrate, reducing galvanic corrosion during calendar aging, enabling the full cell to retain 90.3% capacity over 600 cycles.
Abstract
Scaling up aqueous zinc (Zn)-ion batteries with long cycling stability and calendar life (i.e., long rest periods at open-circuit potential) remains challenging, particularly with the use of a thick Zn foil anode. A more practical and scalable approach involves adopting a lean-Zn configuration with a current collector. Due to the limited Zn availability, lean Zn anodes experience different failure mechanisms, manifested as Zn pulverization in cycle life and galvanic corrosion during calendar life. Unfortunately, these issues have long been overlooked. Herein, we introduce benzotriazole (BTA), a well-known corrosion inhibitor, as an electrolyte additive in aqueous zinc sulfate (ZnSO4) electrolytes. BTA modifies the electric double layer (EDL) structure on the Zn anode, alleviating the mismatch between Zn2 + mass transport and reduction kinetics. This leads to the formation of dense, flat zinc deposits rather than the Zn pulverized structures, significantly reducing contact loss during stripping. On the other hand, the strong chemisorption of BTA on the Cu substrate effectively blocks electron transfer pathways responsible for galvanic corrosion, reducing capacity fade during calendar aging. When paired with a MnO2 cathode, the lean-Zn anode enables the full cell to retain 90.3% of its capacity over 600 cycles at a negative: positive (N:P) ratio of 3:1.
Read the paper
Discussion · 1
Science Skim's AI key points, plus readers' public thoughts
- Benzotriazole (BTA) is introduced as an electrolyte additive in ZnSO4 electrolytes to modify the electric double layer on the Zn anode.
- BTA alleviates the mismatch between Zn2+ transport and reduction kinetics, forming dense zinc deposits and reducing pulverization.
- BTA also blocks electron transfer pathways on the Cu substrate, reducing galvanic corrosion during calendar aging, enabling the full cell to retain 90.3% capacity over 600 cycles.
Readers' thoughts
No reader thoughts yet.
Related papers
- Toward High‐Performance Zn Anodes: A Synergistic Dual‐Ion Strategy via Interfacial Orientation OptimizationAdvanced Functional Materials · 2026
- Cation‐Assisted Zinc Ion Desolvation for Long‐Cycled Zinc Metal Anodes at High Current RatesAdvanced Energy Materials · 2025
- Synergistic Texture Engineering and Grain-Boundary Stabilization for Aqueous Zinc-Ion Batteries With Ultralong Cycling Life Under Extreme Conditions.Small (Weinheim an der Bergstrasse, Germany) · 2026
- Corrosion-resistant organic-inorganic hybrid interphase integrated with nitrile coordination enables highly stable zinc metal anodes.Journal of colloid and interface science · 2026
- Trace‐Level Green Bio‐Derived Amino Acid Molecular Leveling Agent Enables Dendrite‐Free and Long‐Lifespan Zinc Metal AnodesAdvanced Materials · 2025
- Competitive Cationic Adsorption‐Driven Dynamic Electrostatic Shielding Enables Ultra‐Stable Zn Metal AnodesEnergy & environment materials · 2026