Lithium Squarate as Sacrificing Electrolyte Additive for Prelithiation: Case Study in Zero‐Excess Lithium Metal Batteries
Ibrahim Lawal Abdullahi, Anindityo Arifiadi, Alexandros Tsoufios, Nick Fehlings, Silvan Stuckenberg, Lukas Stolz, Dominik Voigt, Martin Winter,
University of Münster · Forschungszentrum Jülich
Key points
From the paper's conclusion- Hence, the squarate is concluded to be impractical as an additive in electrolytes when combined with anodes, which in operando form the SEI (e.g., graphite, Si).
Abstract
Abstract Among different approaches, the prelithiation via sacrificing additives can be technically relatively easy applied. In this work, lithium squarate (Li 2 C 4 O 4 ) as a literature‐known representative is investigated in zero‐excess lithium metal batteries, which are simple in handling and have high active lithium loss (ALL), thus ideal for R&D of sacrificing additives. When incorporated via cathode, Li 2 C 4 O 4 oxidizes at a relatively low cathode potential (≈4.5 V vs Li|Li⁺) and provides the aimed active Li (= capacity), but ruptures the cathode via gaseous evolution of CO and CO 2 . Interestingly, when incorporated via electrolyte, the additive oxidation is absent. This can be correlated with its reductive depletion in the course of solid electrolyte interphase (SEI) formation, as hinted via computational analysis by its relatively low energetic level of lowest unoccupied molecular orbital (LUMO), as well as by energy dispersive x‐ray spectroscopy, and decreased gas evolution. Hence, the squarate is concluded to be impractical as an additive in electrolytes when combined with anodes, which in operando form the SEI (e.g., graphite, Si). In Li metal cells, i.e., with an already existing and passivating “preformed” native SEI, the squarate oxidation can be seen again, but the oxidation onset sensitively depends on the cathode type and electrolyte formulation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Li₂ O‐Integrated Electrodes Enabling Enhanced Adsorption/Defluorination Kinetics Toward LiF‐Rich Interphase for High‐Performance Lithium Metal BatteriesAdvanced Functional Materials · 2025
- Redirecting Bond Cleavage in Sacrificial Prelithiation via Dual‐Side Separator Engineering for Anode‐Free Lithium BatteriesAdvanced Energy Materials · 2026
- Highly stable quasi-solid-state initially anode-free lithium metal batteries enabled by dynamic integrated interface engineering.Nature communications · 2026
- Role-Differentiated Solvation Directs Interfacial Chemistry in Wide-Temperature Lithium Metal Batteries.Angewandte Chemie (International ed. in English) · 2026
- Interfacial Catalytic Activation of Li2C2O4 for Efficient Cathode Prelithiation in Lithium-Ion Batteries.Small (Weinheim an der Bergstrasse, Germany) · 2026
- Revisiting Coulombic Efficiency Paradigm: Electrolyte Additive Design for Lithium Metal BatteriesAngewandte Chemie · 2026