Fluorinated Propyltriphenylphosphonium‐Engineered Moisture‐Stable Manganese Halide Scintillators for High‐Performance X‐Ray Imaging
Zhenjie Huang, Siyin Hu, Kunhua Lai, Jiahui Chen, Shan‐Ci Chen, Mei‐Jin Lin, Huanghao Yang
Key points
From the paper's conclusion- Benefiting from a melting point lower than its decomposition temperature, (C 3 FTPP‐F) 2 MnBr 4 can be further processed into a transparent scintillator glass by melt‐quenching, enabling high‐resolution X‐ray imaging with a spatial resolution of 31.8 lp mm −1 .
Abstract
Zero‐dimensional (0D) manganese‐based organic–inorganic halides are promising lead‐free scintillators because of their high luminescence efficiency, large Stokes shifts, and structural tunability, but their practical use is hindered by poor moisture stability. Herein, we develop a fluorination strategy based on phosphonium‐cation engineering to simultaneously improve the scintillation performance and moisture stability of 0D manganese halides. By introducing fluorine atoms into the phenyl rings and alkyl chain of propyltriphenylphosphonium, three manganese‐based halide scintillators, (C 3 TPP) 2 MnBr 4 , (C 3 TPP‐F) 2 MnBr 4 , and (C 3 FTPP‐F) 2 MnBr 4 , were successfully designed and synthesized. All three compounds exhibit green emission under UV and X‐ray excitation. Among them, (C 3 FTPP‐F) 2 MnBr 4 shows the best overall performance, with a photoluminescence quantum yield of 79.4%, an estimated light yield of 49 000 photons MeV −1 , and a low detection limit of 109.2 nGy s −1 . More importantly, fluorination markedly enhances the moisture stability of the materials. After exposure to 100% relative humidity for 15 days, (C 3 FTPP‐F) 2 MnBr 4 retains about 50% of its initial radioluminescence intensity, whereas the non‐fluorinated analog undergoes rapid degradation and complete luminescence quenching within 3 days. Benefiting from a melting point lower than its decomposition temperature, (C 3 FTPP‐F) 2 MnBr 4 can be further processed into a transparent scintillator glass by melt‐quenching, enabling high‐resolution X‐ray imaging with a spatial resolution of 31.8 lp mm −1 .
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Manganese(II)‐Based Luminescent Materials for Advanced ScintillationAdvanced Functional Materials · 2026
- A Hybrid Manganese Halide Scintillator with a High X-ray Absorption Coefficient for X-ray ImagingInorganic Chemistry · 2026
- Lighting Hidden Traces: Rapid Green Synthesis of Zero-Dimensional Manganese Halide Perovskite for X-Ray and Fingerprint Imaging.Small (Weinheim an der Bergstrasse, Germany) · 2026
- H/F Substitution Regulates the Local Environment and Excited-State Relaxation of Tetrahedral Mn(II) Centers for Near-Unity Luminescence and X-ray Scintillation.Inorganic chemistry · 2026
- Molecular Confinement Engineering of Mn(II) Halide Scintillators for High-Resolution X-ray Imaging and Three-Dimensional Computed Tomography.Inorganic chemistry · 2026
- Concurrently Achieving Excellent Anti‐Thermal Quenching and Ultrahigh Light Yield in Scintillation of Hybrid Manganese HalidesLaser & Photonics Reviews · 2026