Advanced materials (Deerfield Beach, Fla.)

Interface Engineering to Unlock Multi-Electron Sn+/S2- Redox Reaction and High Lithium Anode Utilization.

Ni Zhang, Hanpu Liang, Runming Zeng, Yifan Ni, Taiwu Yu, Shan Zhang, Bao Zhang, Daming Zhu,

Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo, P. R. China. · School of Materials and Energy, University of Electronic Science and Technology of China, Chengdu, P. R. China.

Key points

From the paper's conclusion
  • A dual-interface engineering strategy was employed to construct phase-separated localized electrochemical microreactors (LEMRs) at both electrodes in all-solid-state lithium-sulfur batteries.
  • The optimized cells delivered a capacity retention of 86.3% after 450 cycles at 3.6 mAh cm-2 and 80% after 70 cycles at a high areal capacity of 7.5 mAh cm-2 under a low N/P ratio of 0.78, and achieved an ultra-high areal capacity of 32.8 mAh cm-2.
  • This work highlights the potential of anion chemistry as an effective interface engineering strategy to overcome the kinetics and stability limits of all-solid-state lithium batteries.

Abstract

All-solid-state lithium-sulfur batteries (ASSLSBs) offer high theoretical energy density, yet their practical viability is impeded by sluggish cathodic redox kinetics and uncontrolled anodic dendrite growth. Here, we address these challenges by a dual-interface engineering strategy that exploits halogen anion migration to in situ construct phase-separated localized electrochemical microreactors (LEMRs) at both electrodes. At the cathode, an in situ-formed Li6PS5Cl/LiCl/Li2S-LiI internal LEMR activates the S2-/Sn+ (n ≥1) multi-electron redox reaction beyond the conventional S2-/S0 redox reaction while maintaining structural integrity. Concurrently, at the Li anode, an interfacial LiCl/C@LiI/LiCl-LiI anode LEMR confines Li plating/stripping within the LEMR to suppress lithium dendrites. This dual-LEMR architecture enables the optimized cells to deliver a capacity retention of 86.3% after 450 cycles at 3.6 mAh cm-2 and 80% after 70 cycles at a high areal capacity of 7.5 mAh cm-2 under a low N/P ratio of 0.78, and to achieve an ultra-high areal capacity of 32.8 mAh cm-2. This work highlights the potential of anion chemistry as an effective interface engineering strategy to overcome the kinetics and stability limits of all-solid-state lithium batteries, and provides a versatile framework for advancing high-energy ASSLSBs.

Read the paper

Discussion · 1

Science Skim's AI key points, plus readers' public thoughts

Science SkimAI key points
Pinned
  • A dual-interface engineering strategy was employed to construct phase-separated localized electrochemical microreactors (LEMRs) at both electrodes in all-solid-state lithium-sulfur batteries.
  • The optimized cells delivered a capacity retention of 86.3% after 450 cycles at 3.6 mAh cm-2 and 80% after 70 cycles at a high areal capacity of 7.5 mAh cm-2 under a low N/P ratio of 0.78, and achieved an ultra-high areal capacity of 32.8 mAh cm-2.
  • This work highlights the potential of anion chemistry as an effective interface engineering strategy to overcome the kinetics and stability limits of all-solid-state lithium batteries.

Readers' thoughts

No reader thoughts yet.