Thermodynamically Guided Antisite Ordering Stabilizes Cobalt-Free Ultrahigh-Ni Cathodes.
Tiantian Zhang, Lingfeng Li, Canshang Liu, Sicheng Niu, Yandi Wen, Yixiao Guo, Zongying Wu, Kunfang Wang,
School of Marine Science and Technology, Harbin Institute of Technology, Weihai, China. · Advanced Battery Technology Center, Harbin Institute of Technology, Harbin, China.
Key points
From the paper's conclusion- Here, we address this central stability challenge by developing a thermodynamics-guided defect-engineering strategy that stabilizes spatially correlated Li/Ni antisite configurations in cobalt-free ultrahigh-Ni cathodes.
Abstract
Eliminating Co from ultrahigh-Ni layered cathodes often exacerbates Li/Ni mixing, impeding Li+ transport, amplifying reaction heterogeneity, and accelerating structural degradation. Most strategies focus on minimizing the overall degree of cation mixing, whereas thermodynamic control of antisite spatial organization remains underexplored. Here, we address this central stability challenge by developing a thermodynamics-guided defect-engineering strategy that stabilizes spatially correlated Li/Ni antisite configurations in cobalt-free ultrahigh-Ni cathodes. Density functional theory screening of high-valence dopants reveals that Te6+ exhibits the strongest energetic preference for spatially correlated antisite configurations. This prediction guides the synthesis of LiNi0.948Al0.045Te0.007O2 containing coherent local antisite-ordered superlattice domains. These ordered domains persist after prolonged cycling, strengthen interlayer coupling, suppress H2-H3 phase separation and c-axis contraction, and preserve low-barrier Li+ migration pathways. Local Te-O coordination further stabilizes lattice oxygen and mitigates oxygen-loss-induced surface reconstruction. Consequently, the cathode delivers 185 mAh g-1 at 10 C, retains 96.7% of its initial capacity after 200 cycles at 1 C with a 4.4 V cutoff, and retains 92% of its initial capacity after 100 cycles with a 4.6 V cutoff. These findings establish the spatial organization of defects as a critical design variable for mitigating the stability-transport trade-off in cobalt-free ultrahigh-Ni layered cathodes.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Spinel nanodomains relieve strain and stabilize lattice oxygen in ultrahigh-nickel zero-cobalt cathodeseScience · 2025
- Superlattice Engineering Stabilizes Bulk-to-Surface Microenvironment in Single-Crystalline Ultrahigh-Ni Cathodes.Advanced materials (Deerfield Beach, Fla.) · 2026
- Tuning σ-Type Ni─O Orbital Hybridization for Stable Ultrahigh-Ni Cathodes.Advanced materials (Deerfield Beach, Fla.) · 2026
- Entropy-Engineered Fe-O-Ni Orbital Coupling Enables Durable Co-Free Ni-Rich Layered Cathodes.ACS applied materials & interfaces · 2026
- Machine learning–assisted discovery of outside-in structure Ni-rich cathode with high performanceScience Advances · 2026
- TiO6 as a Compensatory Structural Unit in Co-Free, High-Ni Layered Oxide for Durable Lithium-Ion Batteries.Advanced science (Weinheim, Baden-Wurttemberg, Germany) · 2026