Breaking Lithium Embrittlement in Alloy Anodes Enables Low-Stack-Pressure All-Solid-State Batteries.
Youlong Sun, Lixue Zhou, Tao Liu, Zhen Ding, Xinyi Huang, Yunpeng Li, Qianru Wang, Xiaowei Wu,
Qingdao Industrial Energy Storage Research Institute, Qingdao Institute of Bioenergy and Bioprocess Technology, Chinese Academy of Sciences, Qingdao, China. · College of Chemistry, Chemical Engineering and Materials Science, Shandong Normal University, Jinan, China.
Key points
From the paper's conclusion- The study introduces a nanoscale amorphous structure during lithiation to overcome limited dislocation slip in lithiated intermetallics, which is a cause of high stack pressure in alloy anodes for all-solid-state batteries.
- The NMC83|LPSCl|(InSn4)0.64·(In3Sn)0.36 cell delivers 84.3% capacity retention over 2000 cycles at 4.0 C, and the NMC83||Si full cell sustains over 400 cycles at 5 MPa.
- This strategy of breaking lithium embrittlement can be extended to other alloy anodes (Al-, Sb-, and Bi-containing alloy) in all-solid-state lithium-ion batteries.
Abstract
Alloy anodes (Si, Al, In, and Sn) are exceptionally promising for realizing dendrite-free, high-energy-density all-solid-state lithium-ion batteries (ASSLIBs). However, even soft metals such as Al, Sn, and In form hard and brittle lithiated intermetallics upon lithiation, requiring commercially impractical stack pressures during operation. Here, we overcome limited dislocation slip in lithiated intermetallics arising from directional covalent bonding by introducing a nanoscale amorphous structure during lithiation. This mitigates the high hardness and brittleness of lithiated alloys, reducing the required stack pressure for alloy anodes from ≥30 to ≤5 MPa. The results reveal that atomically mixed In and Sn generate abundant nanoscale amorphous structures during lithiation, as mutual lattice disruption suppresses long-range crystallization. This amorphization facilitates inter-unit sliding and mitigates the effects of directional covalent bonding in intermetallics, thereby reducing their inherent hardness and brittleness. Consequently, the NMC83|LPSCl|(InSn4)0.64·(In3Sn)0.36 cell (cathode areal loading: 22.37 mg cm-2) delivers 84.3% capacity retention over 2000 cycles at 4.0 C. After incorporating (InSn4)0.64(In3Sn)0.36 composite into Si anode, the NMC83||Si full cell sustains over 400 cycles at 5 MPa and is further validated in pouch cells. This strategy of breaking lithium embrittlement can also be extended to other alloy anodes (Al-, Sb-, and Bi-containing alloy) in ASSLIBs.
Read the paper
Discussion · 1
Science Skim's AI key points, plus readers' public thoughts
- The study introduces a nanoscale amorphous structure during lithiation to overcome limited dislocation slip in lithiated intermetallics, which is a cause of high stack pressure in alloy anodes for all-solid-state batteries.
- The NMC83|LPSCl|(InSn4)0.64·(In3Sn)0.36 cell delivers 84.3% capacity retention over 2000 cycles at 4.0 C, and the NMC83||Si full cell sustains over 400 cycles at 5 MPa.
- This strategy of breaking lithium embrittlement can be extended to other alloy anodes (Al-, Sb-, and Bi-containing alloy) in all-solid-state lithium-ion batteries.
Readers' thoughts
No reader thoughts yet.
Related papers
- Interface Stabilization via In Situ Lithiated Sn Interlayer in All‐Solid‐State Li‐Metal Batteries: Toward Pellet‐Type Cell to Pouch‐Type CellAdvanced Energy Materials · 2026
- Engineering a Fast Li+-Diffusion Secondary Phase in Sn Anodes for Low-Pressure All-Solid-State Batteries.Journal of the American Chemical Society · 2026
- Recent advances in alloy anodes for all-solid-state lithium metal batteries.Chemical communications (Cambridge, England) · 2026
- Net-like Al-Si Anode Integrating Structural Anchoring with Built-In 3D Ion Channels for High-Power-Density All-Solid-State Lithium Batteries.ACS applied materials & interfaces · 2026
- Li Atomic Diffusivity: A Key Descriptor for Critical Current Density and Cycling Stability in Alloy Anodes for All-Solid-State Lithium BatteriesJournal of the American Chemical Society · 2025
- Lithium Alloying Strategies for Anode/Solid‐State Electrolyte Interface Engineering in Solid‐State Lithium Metal BatteriesBatteries & Supercaps · 2026