A Sustainable Fully Fluorine‐Free Interfacial Chemistry for Reversible Anode‐Free Lithium Metal Batteries
Xuzhi Duan, Zihuan Min, Lingxi Zhou, Weijian Xu, Jiahui He, Wanqi Zhang, Songxin Lu, Kaicheng Zhang,
Key points
From the paper's conclusion- This work demonstrates the potential of fluorine‐free interfacial engineering for anode‐free lithium metal batteries, while further improvements in lithium‐inventory retention and high‐current‐density operation remain necessary for practical implementation.
Abstract
Anode‐free lithium metal batteries promise high energy density. However, fluorinated electrolytes raise sustainability concerns. Herein, we develop a fully fluorine‐free interfacial strategy by coupling a cross‐linked vinylene carbonate‐N,N′‐methylenebisacrylamide artificial solid electrolyte interphase (ASEI) on Cu current collectors with a fluorine‐free electrolyte to regulate both lithium deposition and subsequent SEI formation. This combination offers an alternative to interfacial stabilization using fluorinated SEI‐forming components or alloy‐forming interlayers. The ASEI possesses strong Li‐ASEI interactions and enhanced lithiophilicity, thereby enabling homogeneous and compact Li deposition with reduced growth overpotential. Furthermore, the ASEI induces the formation of a conformal, mechanically robust, inorganic‐rich SEI containing Li 2 O and Li 3 N, leading to improved interfacial stability and the reversibility of Li plating/stripping. Consequently, the ASEI‐modified current collector delivers markedly improved full‐cell performance. The prelithiated LFP||ASEI‐Cu full cell achieves stable cycling over 350 cycles with a capacity retention of 84.5% at 25°C, while the prelithiated NCM811||ASEI‐Cu full cell delivers a reversible capacity of 146.8 mAh g −1 after 100 cycles with a capacity retention of 86.6% at 25°C. This work demonstrates the potential of fluorine‐free interfacial engineering for anode‐free lithium metal batteries, while further improvements in lithium‐inventory retention and high‐current‐density operation remain necessary for practical implementation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Highly stable quasi-solid-state initially anode-free lithium metal batteries enabled by dynamic integrated interface engineering.Nature communications · 2026
- Toward practical anode-free lithium batteries through planar deposition and interphase engineeringEnergy Z · 2026
- Fluorine-free gel polymer electrolyte for lithium oxide-rich solid electrolyte interphase and stable Li metal batteriesNature Communications · 2025
- Stable 4.6 V Anode‐Free Li Metal Batteries Enabled by Orchestrating Direct and Indirect Pre‐LithiationAdvanced Functional Materials · 2026
- Li₂ O‐Integrated Electrodes Enabling Enhanced Adsorption/Defluorination Kinetics Toward LiF‐Rich Interphase for High‐Performance Lithium Metal BatteriesAdvanced Functional Materials · 2025
- A self-assembled monolayer regulates solid electrolyte interphase formation in anode-free lithium metal batteries.Nanoscale · 2026