Interfacial Evolution, Failure Mechanisms, and Multiscale Stabilization Strategies for Silicon Anodes in Sulfide‐Based All‐Solid‐State Batteries
Huikun Liu, Zhixiao Yin, Shuai Wang, Yangzhou Ma, Hailiang Deng, Cuie Wen, Guangsheng Song
Key points
From the paper's conclusion- The review discusses the challenges of using silicon anodes in sulfide-based all-solid-state batteries, including structural reconstruction, volume variation, and interfacial instability during cycling.
- Interphase growth, loss of active lithium, particle fracture, interfacial delamination, contact loss, and heterogeneous ionic/electronic transport lead to electrochemical–chemical–mechanical degradation.
- Stabilization strategies such as structural regulation, carbon hybridization, conductive-network construction, and pressure management are critically assessed to address these degradation mechanisms.
Abstract
Silicon anodes offer exceptionally high theoretical capacity and low lithiation potential, making them attractive for high‐energy‐density all‐solid‐state batteries using sulfide solid‐state electrolytes. However, Si undergoes substantial structural reconstruction and volume variation during cycling, while deeply lithiated Li x Si strongly reduces sulfide solid‐state electrolytes. The resulting interphase growth, loss of active lithium, particle fracture, interfacial delamination, contact loss, and heterogeneous ionic/electronic transport produce tightly coupled electrochemical–chemical–mechanical degradation. This Review summarizes the alloying‐type Li‐storage mechanism and room‐temperature phase evolution of Si, emphasizing low‐potential interfacial instability, volume‐strain‐induced fracture, solid–solid contact loss, and pressure‐dependent failure. Stabilization strategies based on structural regulation, carbon hybridization, conductive‐network construction, prelithiation, Li–Si alloying, elemental doping, surface modification, protective interlayers, functional binders, electrode processing, and pressure management are critically assessed. Advanced characterization and modeling methods are discussed for resolving interfacial reactions and failure pathways. Future progress requires chemically stable and mechanically compliant interfaces, low‐pressure architectures, controllable prelithiation, scalable manufacturing, artificial‐intelligence‐assisted design, standardized full‐cell evaluation, and coordinated optimization of transport, stress accommodation, Li inventory, and manufacturability.
Read the paper
Discussion · 1
Science Skim's AI key points, plus readers' public thoughts
- The review discusses the challenges of using silicon anodes in sulfide-based all-solid-state batteries, including structural reconstruction, volume variation, and interfacial instability during cycling.
- Interphase growth, loss of active lithium, particle fracture, interfacial delamination, contact loss, and heterogeneous ionic/electronic transport lead to electrochemical–chemical–mechanical degradation.
- Stabilization strategies such as structural regulation, carbon hybridization, conductive-network construction, and pressure management are critically assessed to address these degradation mechanisms.
Readers' thoughts
No reader thoughts yet.
Related papers
- Silicon‐Based Anodes for Sulfide Solid‐State Batteries: Failure Mechanisms and Multiscale Design StrategiesAdvanced Energy Materials · 2026
- Decoupling Chemo‐Mechanical Degradation for Scalable Silicon‐Based Solid‐State BatteriesAdvanced Materials · 2026
- Interfacial engineering in sulfide-based all-solid-state batteries: from cathode/anode interfaces to electrolyte modification.Chemical science · 2026
- Coupled Design of Silicon Anodes and Solid-State Electrolytes for High-Performance All-Solid-State Batteries.ACS nano · 2026
- Interface-Mediated Architectural Engineering of Silicon for Solid-State Batteries: Current Status and Future Outlook.Advanced materials (Deerfield Beach, Fla.) · 2026
- High-Performance All-Solid-State Silicon-Sulfur Batteries Enabled by Li4(BH4)3I Hydride Electrolyte.Small (Weinheim an der Bergstrasse, Germany) · 2026