Dual‐Sided Regulation of Lithium Deposition for High‐Energy‐Density Anode‐Less Lithium Metal Batteries
Jisub Kim, Jong Min Won, Gaeun Park, Kunik Jang, Green Baek, Seohan Ji, Sangjin Bae, Seung Woo Lee,
Key points
From the paper's conclusion- A dual-sided regulation strategy was developed to homogenize lithium (Li) deposition in anode-less Li metal batteries by implementing an ultrathin platinum (Pt) layer at the current collector and an amorphous tantalum oxide (a-TaOx) ceramic layer at the separator.
- The Pt/a-TaOx dual-interface design enabled stable cycling with 70% capacity retention after 110 cycles in an anode-less configuration (N/P ratio = 0) and 80% after 187 cycles with pre-lithiation (N/P ratio = 0.42).
- This approach establishes a new framework for stabilizing Li deposition across the full thickness in high-capacity anode-less Li metal batteries by transcending conventional bottom-only protection.
Abstract
Anode‐less lithium (Li) metal batteries are the ultimate anode configuration for high‐energy‐density energy storage, yet their practical adoption is hindered by uncontrolled Li dendrite growth. Here, we present a dual‐sided regulation strategy that homogenizes Li deposition through simultaneous bottom‐up and top‐down control. At the current collector, an ultrathin platinum (Pt) layer leverages its lithiophilicity to stabilize nucleation and promote dense bottom growth. At the separator, an amorphous tantalum oxide (a‐TaO x ) ceramic layer exploits thermodynamic Li dewetting to suppress upward dendritic propagation, enforcing top‐down uniformity. This synergistic Pt/a‐TaO x dual‐interface design orchestrates Li deposition across the entire electrode, enabling stable cycling at high cathode areal capacities (4.78 mAh cm– 2 ) with 70% capacity retention after 110 cycles in an anode‐less configuration (N/P ratio = 0) and 80% after 187 cycles with pre‐lithiation (N/P ratio = 0.42). By transcending conventional bottom‐only protection, this work establishes a new framework for stabilizing Li deposition across the full thickness in high‐capacity anode‐less Li metal batteries.
Read the paper
Discussion · 1
Science Skim's AI key points, plus readers' public thoughts
- A dual-sided regulation strategy was developed to homogenize lithium (Li) deposition in anode-less Li metal batteries by implementing an ultrathin platinum (Pt) layer at the current collector and an amorphous tantalum oxide (a-TaOx) ceramic layer at the separator.
- The Pt/a-TaOx dual-interface design enabled stable cycling with 70% capacity retention after 110 cycles in an anode-less configuration (N/P ratio = 0) and 80% after 187 cycles with pre-lithiation (N/P ratio = 0.42).
- This approach establishes a new framework for stabilizing Li deposition across the full thickness in high-capacity anode-less Li metal batteries by transcending conventional bottom-only protection.
Readers' thoughts
No reader thoughts yet.
Related papers
- Anode-Less (Anode-Free) Batteries: From Fundamental Principles to Practical Pathways Toward Solid-State ImplementationMaterials · 2026
- Interfacial Chemo-Mechanical Engineering of a Vertically Aligned Host for Reversible Anode-Less Lithium Metal Batteries.Small (Weinheim an der Bergstrasse, Germany) · 2026
- In situ anchoring 2D hexagonal Zn-MOF on MXene toward robust anode-less 5 V–class Li metal batteriesScience Advances · 2026
- Redirecting Bond Cleavage in Sacrificial Prelithiation via Dual‐Side Separator Engineering for Anode‐Free Lithium BatteriesAdvanced Energy Materials · 2026
- Recent Advances in Lithium Metal Anodes with Liquid Electrolytes: Interfacial Interaction‐Driven Assembly for Dendrite Suppression and Long‐Term StabilitySmall · 2026
- Strain Coupled (110)-Oriented Lithium Anodes for High-Rate and High-Capacity Epitaxial Growth.ACS nano · 2026