Dual‐Interphase Engineering With Nano‐Alumina and CVD Carbon Enabling High‐Temperature Calendar Aging Mitigation in Silicon‐Oxide Anode
Lifu Chen, Lezhi Yang, Wei‐Li Song, Yunfeng Liu, Tao Chen, Shuang Wang, Zhengguo Gu, Buwen Shi,
Changsha Mining and Metallurgy Research Institute (China) · Hunan Normal University
Key points
From the paper's conclusion- The stability of high‐temperature storage in silicon‐based high‐energy lithium‐ion batteries (LIBs) is highly critical.
- A strategy of solid‐state mechanofusion‐chemical vapor deposition (SSM‐CVD) is proposed to construct a dual‐phase nano‐alumina (Al 2 O 3 ) and dense carbon on the micron‐sized silicon oxide (SiO) particles (SiO@Al 2 O 3 /C).
- The capacity retention reaches 97.81% with a capacity recovery rate of 99.46% in the as‐assembled commercial 18 650 cylindrical cells after high‐temperature storage (60°C for 14 days).
Abstract
ABSTRACT The stability of high‐temperature storage in silicon‐based high‐energy lithium‐ion batteries (LIBs) is highly critical in the operation temperature beyond 40°C, typically in tropical and subtropical regions globally. The unexpected stability of high‐temperature storage would lead to severe self‐discharge, which accelerates the decay of remaining capacity, side reaction‐induced electrolyte decomposition, and fire‐hazard risk. To address such issues, a strategy of solid‐state mechanofusion‐chemical vapor deposition (SSM‐CVD) is proposed to construct a dual‐phase nano‐alumina (Al 2 O 3 ) and dense carbon on the micron‐sized silicon oxide (SiO) particles (SiO@Al 2 O 3 /C), with the purpose of suppressing the self‐discharge behavior induced by charge transfer between graphite (Gr) and SiO in the negative electrode. With the presence of such dual‐phase coating, a stable solid electrolyte interphase has been constructed on both SiO@Al 2 O 3 /C and graphite. The electrochemical performance at high‐temperature storage (60°C for 14 days) suggests that the capacity retention reaches 97.81% with a capacity recovery rate of 99.46% in the as‐assembled commercial 18 650 cylindrical cells, which approaches a record‐setting value under the severe high‐temperature storage condition. This work also elucidates high‐temperature failure mechanisms and offers an SSM‐CVD engineering strategy for stabilizing both capacity and safety in silicon‐based high‐energy LIBs.
Read the paper
Discussion · 1
Science Skim's AI key points, plus readers' public thoughts
- The stability of high‐temperature storage in silicon‐based high‐energy lithium‐ion batteries (LIBs) is highly critical.
- A strategy of solid‐state mechanofusion‐chemical vapor deposition (SSM‐CVD) is proposed to construct a dual‐phase nano‐alumina (Al 2 O 3 ) and dense carbon on the micron‐sized silicon oxide (SiO) particles (SiO@Al 2 O 3 /C).
- The capacity retention reaches 97.81% with a capacity recovery rate of 99.46% in the as‐assembled commercial 18 650 cylindrical cells after high‐temperature storage (60°C for 14 days).
Readers' thoughts
No reader thoughts yet.
Related papers
- Thermochemical Core-Shell Architecturing of Si-SWCNT Composites for High-Performance Li-Ion Battery Anodes.Advanced science (Weinheim, Baden-Wurttemberg, Germany) · 2026
- 4.5‐V‐Class Safe Lithium‐Ion Batteries with Silicon‐Majority‐Graphite Anodes Enabled by Self‐Limiting InterphaseAdvanced Materials · 2025
- Tailoring Sieving Pores and Electrochemical Interface Intercalation for Mechanically Resilient Recycled Micro‐Silicon AnodesAdvanced Science · 2025
- High–performance recycled silicon–based Li–ion battery anodes enabled by Si/C composites engineering and graphene oxide protective layerJournal of Power Sources · 2025
- Hierarchical Carbon-Al2O3 Reaction Boundary Regulates Electrolyte-Dependent Interphase Evolution in Photovoltaic-Waste Silicon Anodes.Molecules (Basel, Switzerland) · 2026
- Stress-adaptive conductive network and ion-segregated polymeric-inorganic interphases enable durable room-temperature silicon-based solid-state batteries.Nature communications · 2026