Advanced Engineering Materials

Lamellar Ti–Ta Alloys by Hot‐Press Sintering: Interface Strengthening, Low Modulus, and Enhanced Corrosion Resistance

Ye Ma, Shidan Yuan, Tingting Li, Ningning Guo, Ze Li, Jinwei Zhang, JunYe Liu, Hui Yang

Key points

From the paper's conclusion
  • Ti–30Ta exhibited optimal corrosion resistance in simulated body fluid, attributed to its nearly equal α/β phase fractions and formation of a continuous TiO 2 –Ta 2 O 5 passive film.

Abstract

Ti–Ta alloys are promising candidates for load‐bearing orthopedic implants owing to their excellent biocompatibility and tunable mechanical properties, yet their high fabrication cost and insufficient strength remain challenging. Here, fully dense Ti–xTa (x = 20, 25, 30, and 35 wt%) alloys with lamellar microstructures were fabricated by a facile and cost‐effective hot‐pressing sintering route at 1300 °C under 30 MPa. With increasing Ta content, the β‐phase fraction increased from 17.1% to 55.8%, while the α phase evolved from a continuous matrix into discrete lamellar and acicular morphologies. The α/β interfaces obeyed the Burgers orientation relationship, forming low‐energy semi‐coherent boundaries that promoted effective interface strengthening. Tensile tests demonstrated enhanced strength and reduced elastic modulus with increasing Ta content, with Ti–30Ta exhibiting an ultralow modulus of 60 GPa. Quantitative modeling confirmed interface strengthening as the dominant hardening mechanism, with yield‐strength prediction errors below 11% for Ti–20Ta to Ti–30Ta. Ti–30Ta exhibited optimal corrosion resistance in simulated body fluid, attributed to its nearly equal α/β phase fractions and formation of a continuous TiO 2 –Ta 2 O 5 passive film. This work provides a scalable strategy for high‐performance Ti–Ta orthopedic implants.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Lamellar Ti–Ta Alloys by Hot‐Press Sintering: Interface Strengthening, Low Modulus, and Enhanced Corrosion Resistance — Science Skim